1) drawability
深冲性
2) deep drawability
深冲性能
1.
The effects of processing parameters of ferritic rolling on microstructures and mechanical properties especially on deep drawability of ultra-low carbon and Ti-stabilized interstitial-free steels were investigated,and the precipitates in Ti-IF steel were also analyzed.
本文研究了铁素体区轧制工艺条件对超低碳(ULC)钢和钛处理的无间隙原子(Ti-IF)钢组织和性能,特别是对深冲性能的影响,并分析了Ti-IF钢中的析出物。
2.
The cross-section metallurgic structure at various annealing temperature is analyzed and compared with import material based on the statistical study of the influence of annealing temperature on the deep drawability of cold rolled IF steel.
在统计分析退火温度对冷轧 IF 钢深冲性能的影响的基础上,对不同退火温度下的断面金相组织亦进行了分析,并与进口料进行了对比。
3) drawability
深冲性能
1.
The effect of the reduction in cold rolling IF steel sheet for drawability;
冷轧压下率分配对IF钢深冲性能的影响
2.
The results showed that the IF steel has better deep drawability,higher mechanical and texture strength and elongation if the hot rolling temperature was low with big reduction in ferrite region.
结果表明,较低的铁素体轧制温度和较高的铁素体区压下量时,IF钢具有更高的深冲性能、相对较高的强度、延伸率以及织构强度。
3.
How the processing conditions affect the properties especially the drawability of a ferritic hot-rolled and annealed Ti-IF sheet steel was investigated.
研究了铁素体轧制工艺条件对一种Ti-IF钢的性能,特别是深冲性能的影响。
4) deep-drawing property
深冲性能
1.
Effect of cold rolling-process on microstructure and deep-drawing property of 1050H19 aluminum foils used in air-conditioner;
冷轧工艺对1050H19空调箔微观结构及深冲性能的影响
2.
The relationship of deep-drawing property and rolling parameters of IF steel was researched by the testing of ferritic rolling and annealing.
通过对IF钢铁素体区轧制、退火工艺的研究及对塑性应变比r值的检测,并结合对取向分布函数图的定量分析,研究了深冲性能与轧制工艺参数的关系。
5) deep drawing property
深冲性能
1.
Influence of texture in 3104 Aluminum sheet on r values and deep drawing property;
3104铝板织构对r值及深冲性能的影响
2.
Functional relationship between deep drawing property and process parameters of Zn-Cu alloy was studied by regression analysis method.
采用回归分析方法研究了Zn-Cu合金深冲性能与工艺参数间的函数关系。
3.
After being rolled in ferrite area, the IF steel was proceeded once and twice cold rolling, then its deep drawing property was studied.
研究了经铁素体区热轧后的 IF钢板坯在随后的一次冷轧和两次冷轧工艺中所表现出的深冲性能规律。
6) deep drawing properties
深冲性能
1.
Under the laboratory condition,by the precipitate observation,the precipitate behavlour of IF-HSS was investigated a new precipitate TiFeP was discovered,and effect of P element in steel on deep drawing properties was further discussed.
高强IF钢是汽车用深冲钢板中深冲性能最好的高强度钢板。
参考词条