1) forming path
成形路径
1.
The theory and method on the blank design, determination of forming path and transition area design of sectional forming in MPF are introduced.
本文介绍了板材多点成形技术中初始坯料设计、成形路径确定以及多点分段成形过渡区设计的有关理论与方法。
2.
In the technique, the functions such as choosing forming path and sectional forming for sheet metal, which can't be realized in traditional method, can be implemented easily.
多点柔性成形是一种先进的金属板材成形技术 ,这种成形方法能够实现成形路径选择、分段成形等传统成形方法无法实现的功能 。
2) pathway
[英]['pɑ:θweɪ] [美]['pæθ'we]
形成路径
1.
Research on the pathway of forming outsourcing network;
资源外包网络的形成路径研究
3) Optimum forming path
最优成形路径
4) path generating
路径生成
1.
In this paper,a laser scanning path generating algorithm is proposed,which is well used in our SL machine.
本文提出了一种简捷有效的扫描路径生成算法,成功地应用于开发的快速成型机中。
5) growth path
成长路径
1.
Research on the growth path of technical capability of automobile manufacture enterprise in later-development countries;
后发国家汽车制造企业技术能力成长路径研究
2.
An analysis on enterprise durative growth path based on the dynamic equilibrium of innovation ability and control ability;
基于创新力与控制力动态均衡的企业持续成长路径分析
6) growing path
成长路径
1.
Research on Growing Path of Small and Medium-Sized Enterprise Cluster in Southwest of China;
西南地区城镇中小企业集群成长路径研究
补充资料:主要射出成形材料成形时应注意事项
■主要射出成形材料成形时应注意事项
品 名 注 意 事 项
PVC
聚氯乙烯
1. 产品种类范围非常广(硬质、软质、聚合物等),成型条件各有不同,从熔融至分
解之温度范围很小,尤须注意加热温度。
2. 附着水分少,但成型周期尽可能减少(50℃~60℃热风干燥)。
3. 成型机方面,与材料直接接触的部位须电镀或采用不锈钢以防热分解所产生的盐酸
侵蚀。射出压力2100kg/cm2程度。
4. 所有塑料当中必须是细心注意温度调节。
5. 浇口附近易产生流纹,故射出操作后,柱塞不要后退使浇口充分固化后再瞬间退后为宜。
6. 加热之初温不宜高,特别注意熔融情形。第二级加热温度较高,且尽可能使成形周
期缩短,比较安全。
PA
聚醯胺树脂
1. 成型温度比其它材料高,故采用油加热的成形机较适当。
2. 吸湿性大,必须充分干燥。水分对成型品的品质影响甚大(80℃热风干燥约5~6小时)。
3. 须退火以消除内部歪斜。
PP
聚丙烯
1. 同PE,但成形温度必须较高。熔融温度170℃,超过190℃则流动性大增,则毛边增加,
易产生接缝及凹入情形。
PC
聚碳酸脂
1. 吸湿性比尼龙小,但若有些微之水分存在则成型品产生其它色泽或气泡,故必须密封
干燥同时成形时也须预备干燥(120℃之温度4小时)。
2. 加热温度超过320℃时则产生热分解,成品变色,故特别注意温度调节,又成型时的温度调节也非常重要,须特别注意其最低温度、最低时间。
3. 须退火以消除内部歪斜(130℃~135℃,1小时程度为准)。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。