1) relative rate of toughness enlargement
相对增韧率
2) Ductile-phase toughening
韧相增韧
3) Relative growth rate
相对增长率
1.
Curve of biomass accretion,absolute growth rate and relative growth rate show "Z" type,of which are 238.
75 g/m2;生物量生长量、生物量绝对增长率和相对增长率季节动态都呈"Z"型,其最大值出现在7月末,分别为238。
2.
As the results show,the daily average relative growth rate of Enteromorpha prolifera is 3.
结果显示,青岛近岸海水不添加营养盐的对照组,浒苔平均每天的相对增长率3。
4) relative increasing rate
相对增长率
1.
Then the relative increasing rates and the relative contents of Chlorophyll(a)were determined.
叶绿素 a含量与各自的相对增长率呈一定的正相关。
5) weight gain
相对增重率
1.
After eight weeks feeding,weight gain,length gain,feed conversion rate,and protein efficiency ratio of common carp were determined.
54)g 8周,测定实验鱼的体长、体重,并计算存活率、相对增重率、相对增长率、饲料系数和蛋白质效率。
6) transformation toughening
相变增韧
1.
The transformation toughening of AT30 and the study on their abrasive wear properties;
AT30金属陶瓷的相变增韧及其对磨粒磨损性能研究
2.
The transformation toughening,mechanisms are surveyed for ZrO 2 ceramics and introduces its types, properties,application in ceramics and other industrial fields.
综合论述了国内外对ZrO2 陶瓷的相变增韧机理的研究 ,介绍了ZrO2 陶瓷的类型和性能以及在陶瓷和其它工业领域的应用前景。
3.
Microcrack toughening and some degree of transformation tougheninghave been achieved by varying amounts of Y_2O_3 addition to adjust the degrees of t-ZrO_2 stabilizationin zirconia toughened mullite (ZTM) composites.
调节氧化锆相中稳定剂Y_2O_3的固溶量可在ZTM复合材料中实现微裂纹增韧和一定程度的相变增韧。
补充资料:氧化锆相变增韧陶瓷
分子式:
CAS号:
性质:一种利用氧化锆马氏体相变效应来改善脆性的陶瓷。氧化锆在由四方相向单斜相转变时(即马氏体相变),伴随体积和形状变化。能吸收能量,减缓裂纹尖端的应力集中,阻止裂纹扩展,从而提高材料韧性,包括应力诱导相变增韧、裂纹弯曲增韧和微裂纹增韧。分为稳定氧化锆陶瓷(PSZ)、四方氧化锆多晶体陶瓷(TZP)和氧化锆增韧陶瓷(ZTC)三种。用于增强陶瓷基和金属基复合材料韧性。
CAS号:
性质:一种利用氧化锆马氏体相变效应来改善脆性的陶瓷。氧化锆在由四方相向单斜相转变时(即马氏体相变),伴随体积和形状变化。能吸收能量,减缓裂纹尖端的应力集中,阻止裂纹扩展,从而提高材料韧性,包括应力诱导相变增韧、裂纹弯曲增韧和微裂纹增韧。分为稳定氧化锆陶瓷(PSZ)、四方氧化锆多晶体陶瓷(TZP)和氧化锆增韧陶瓷(ZTC)三种。用于增强陶瓷基和金属基复合材料韧性。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。