1)  Repairing material
补炉砂
2)  fettling
补炉
1.
Some measures have been taken to prolong tapping hole life greatly such as optimizing heat exchange process,changing the structure of tapping hole,improving properties of fettling materials and decreasing tapping temperature and so on.
通过采取优化出钢口热换工艺、改变出钢口结构材质、优化补炉料性能、降低出钢温度等措施,提高出钢口寿命。
2.
Some measures have been taken to maintain the furnace condition such as optimizing smelting operation,intensifying slag splashing and improving the method of fettling.
转炉炉壁厚达到300mm左右时进入炉役后期,通过优化冶炼操作、强化溅渣护炉、补炉方法维护炉况,实现冶炼品种钢的目的,取得了明显效果。
3)  fettling
大补炉
1.
The phosphorus content in the first heat steel of converter steelmaking after fettling was higher than normal operation and some times even higher than the standard limitation.
转炉大补炉后冶炼第一炉钢时钢中磷含量容易偏高, 有时甚至超出钢种要求的磷含量上限。
4)  fettling mix for converter
补炉料
1.
Physical and chemical properties of industrial slag containing TiO2 is analyzed,and material properties of the fettling mix for converter such as density,strength,high-temperature stability and slag corrosion resistance are studied afrer adding industrial slag containing TiO2 into fettling mix for converter.
分析了含TiO2工业渣的物理化学特性,研究了在耐火补炉料中加入含TiO2工业渣后对材料的体积密度、强度、高温体积稳定性、抗熔渣侵蚀等性能的影响。