说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> TCP相含量
1)  TCP phase amount
TCP相含量
2)  TCP phase
TCP相
1.
After 500h,TCP phase was not foun.
结果表明:随着Ti含量的增加,铸态组织中枝晶间区域面积以及枝晶间区域的γ/γ′共晶含量逐渐增加;长期时效后随着Ti含量的增加,筏形化程度越来越严重,逐渐有TCP相析出。
2.
Results show that the elements W and Re may promote the precipitation of TCP phase.
结果表明:元素W、Re可促进TCP相的析出,合金在1100℃长期时效期间,TCP相沿{111}晶面<110>方向以共格方式析出,在不同晶面多组针状TCP相可相互垂直、或互成60o角排列,并确定出析出的TCP相为μ相。
3.
In this paper,by means of Md and Nv method,five kinds of nickel-based superalloy compositions have been designed to predict the tendency of TCP phase precipitated.
本文采用Md法和Nv法预算了5种镍基合金TCP相的析出倾向,通过对合金进行长期时效及组织形貌观察,研究了含Re合金中TCP相的演化规律;通过X-射线衍射分析及单晶镍基合金蠕变曲线的测定,研究了元素Re含量对合金晶格常数及错配度的影响及单晶合金的蠕变行为。
3)  TCP phase
TCP 相
1.
At the same time,the TCP phase appeared in the grain.
试验结果表明,随着时效时间的延长,碳化物从晶界断续的析出转变为连续的析出,并且晶内有 TCP 相出现,合金的断裂韧性降低,断裂方式由混合型断裂转变为沿晶断裂。
4)  solid loading
固相含量
1.
Gelcasting was applied to shaping of titanium alloy(Ti6Al4V) powders and the preparation of titanium alloy powder’s slurries with high solid loading was investigated.
将凝胶注模工艺应用于金属Ti6Al4V合金粉末的成形,研究了高固相含量的Ti6Al4V合金粉末的料浆的制备,比较了金属浆料与陶瓷浆料的不同。
2.
Thedependence of AT suspension rheological properties on various solid loading and different dispersants wasstudied,and the influence of monomer(AM) and cross-linking agent(MBAM) content on properties of ATbodies was also discussed.
研究了分散剂和固相含量对钛酸铝浆料流变性的影响,并探讨了单体和交联剂用量对钛酸铝坯体性能的影响规律。
3.
The preparation of titanium alloy powder's slurries with high solid loading was investigated.
将凝胶注模工艺应用于金属Ti及Ti-6Al-4V合金粉末的坯体成形,研究了高固相含量的Ti粉和Ti-6Al-4V合金粉末的料浆的制备。
5)  solids loading
固相含量
1.
The influences of solids loading on the rheological properties used for aqueous gel-casting were studied, and also in this paper the microstructures, densities, and strengths of yttria-stabilized zirconia were investigated.
主要研究料浆固相含量对氧化钇稳定氧化锆料浆流变性质,以及YSZ的微结构、密度和强度的影响规律,并分析讨论其原因。
6)  relative content
相对含量
1.
Determination of molecular weight and relative content of the Component of polysaccharide krestin with aqueous gel permeation chromatography;
水溶性凝胶渗透色谱测定芸芝多糖各组分的分子量及相对含量
2.
The relative content of SiC in samples increases gradually with the increasing mole ratio of SiO_2 to C.
随着n(C)∶n(SiO2)的增加,产物中SiC的相对含量逐渐增大。
3.
The study collected volatile gas from leaves and wood of 5 Taxodiaceae species: Crytomeria fortunei,Cumminghamia lanceolata,Metasequoia glyptostroboedes,Taxodium ascendeus and Taxodium distinchum,in Nanyue, Jin an,Lin an,and analyzed the chemical components and their relative content in the volatile gas by GC/MS/DS.
为了解杉科植物所含精气的化学成分及其相对含量,在湖南南岳、江西靖安、浙江临安选择柳杉、杉木、水杉、池杉和落羽杉5个树种的纯林采集各树种的叶片和木材释放的精气,采用气相色谱/质谱联机法分析、鉴定其所含化学成分及其相对含量。
补充资料:2,4,6-TCP
分子式:C6H3Cl3O
分子量:197.45
CAS号:88-06-2

性质:密度1.49。熔点65-68°C。沸点246°C。闪点99°C。水溶性0.8 g/L。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条