1) aluminum cell of self-bake
自焙电解槽
1.
This paper discusses the technological plan to cleaner production of 75kA aluminum cell of pre-bake which is reconstructed from the present 60kA aluminum cell of self-bake.
提出了利用现有的 6 0kA自焙电解槽改建成 75kA预焙电解槽清洁生产工艺方案 ,并将改建前后产品产量、排污、能耗进行对比。
2) horizontal studpor
铝电解自焙槽
3) cell with self baking anode
自焙阳极电解槽
4) side insert self-baking cells
侧插自焙电解槽
1.
This paptr introduced with emphases energy saving management experience and examination measures about 60kA side insert self-baking cells.
本文着重介绍我厂60kA侧插自焙电解槽节能降耗的管理经验和考核措施,节能降耗效果明显。
5) soederberg cell with side studs
侧插自焙阳极电解槽
6) horizontal stud soderberg cells
侧插自焙铝电解槽