1) Cr12 wear-resistant cast iron
Cr12耐磨铸铁
1.
Here the quenching treatment of the Cr12 wear-resistant cast iron is carried out.
将量化水淬技术应用在Cr12耐磨铸铁工件上 ,极大地提高工件的硬度及使用寿命 ,实现高Cr耐磨铸铁的水淬处理。
2) wear resistant cast iron
耐磨铸铁
1.
High chromium molybdenum tungsten wear resistant cast irons are well known for its high hardness.
高铬钼钨耐磨铸铁以高硬度著称。
2.
RE modification followed by heat treating will obtain more noticeable effect for the wear resistant cast iron.
研究了稀土变质处理对耐磨铸铁显微组织及冲击韧性的影响。
3) high chromium wear resistant and corrosion resistant cast iron
耐磨耐蚀铸铁
1.
By the use of metallurgical microscope and scanning electron microscope (SEM), this paper studies the effects of Cr/C on the microstructure of high chromium wear resistant and corrosion resistant cast iron with 4 percent of nickel.
文中利用金相显微镜、扫描电镜(SEM),探讨了Cr/C对含4%Ni耐磨耐蚀铸铁组织的影响规律。
4) Cr12 Ferrite Heat Resistant Steel
Cr12铁素体耐热钢
5) high alloy wear-resistant cast iron
高合金耐磨铸铁
1.
The effect of heating temperature on abrasion resistance of high alloy wear-resistant cast iron was studied.
研究了加热温度对高合金耐磨铸铁耐磨性的影响。
6) low alloy wear resistant cast iron
低合金耐磨铸铁
1.
The influence of heating temperature on impact toughness of low alloy wear resistant cast iron bearing with rare earth elements was studied by means of metallographic examination,scanning electron microscopic examination and mechanical property test.
采用金相、扫描电镜和力学性能分析方法研究了加热温度对含稀土低合金耐磨铸铁冲击韧性的影响。
2.
Aimed at the eutectic carbides distributed at network shape in the cast iron,the effect of heat treatment on morphology of eutectic carbides in low alloy wear resistant cast iron after deformation was studied.
针对低合金耐磨铸铁组织中共晶碳化物呈连续网状分布问题,探讨了热处理对变形低合金耐磨铸铁中共晶碳化物形态的影响。
3.
The influence of heating temperature on morphology of eutectic carbide and impact fatigue property of low alloy wear resistant cast iron were studied by OM, SEM and impact fatigue tester.
采用金相显微镜、扫描电镜及冲击疲劳试验机研究了加热温度对低合金耐磨铸铁中共晶碳化物形态和冲击疲劳性能的影响。