1) critical cooling rate of bainite start point
贝氏体开始转变临界冷却速度
3) bainite start temperature
贝氏体转变开始温度
1.
The results indicate that bainite start temperature decreases with the raising of cooling rate and increases with the increasing of deformation temperature.
研究表明,在连续冷却条件下,随着冷却速度的增加,贝氏体转变开始温度降低。
4) critical cooling rate
临界冷却速度
1.
The critical cooling rates in undercooled austenite transformation process of T91 ferritic heat-resistant steel were studied by DIL805A/D high-resolution differential dilatometer.
利用DIL805A/D高精度差分膨胀仪,通过线膨胀行为测量与微观组织分析,获得T91铁素体耐热钢连续冷却转变过程中相关动力学信息,结合冷却后T91钢组织特征,确定了T91钢过冷奥氏体转变过程中的临界冷却速度。
2.
The critical cooling rate determined by DTA method is 7.
以基于DTA的合金凝固点偏移的方法确定该合金的临界冷却速度Rc=7。
3.
A concept of critical cooling rate given in this paper for carburizing and post heat treatment of steel.
在解决该问题的过程中 ,提出了一个临界冷却速度的概念 ,对钢的渗碳及其后热处理有重要的指导意
5) upper critical cooling velocity
上临界冷却速度
6) martensite start temperature M s
马氏体开始转变温度MS
1.
The formula to calculate the martensite start temperature M s is a liner equation at present.
计算马氏体开始转变温度MS 的公式 ,目前为直线方程式。