说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 原位内生
1)  In situ
原位内生
1.
Study on In situ V_8C_7 Particle Reinforced Iron Matrix Surface Composite;
原位内生碳化钒颗粒增强铁基表面复合材料的研究
2)  in-situ regeneration
原位再生,体内再生
3)  In-situ Synthesis
原位生成
1.
Study of in-situ synthesis of TiB_2by laser cladding and its microstructure;
激光熔覆原位生成TiB_2及其组织结构研究
2.
The carburising reaction of V to form VC take place under solid phase sintering at 850 ℃, and the in-situ synthesis VC particulate is fine, so the size is smaller than 0.
讨论了烧结温度对VC颗粒大小和分布的影响,在850℃固相烧结时,钒的碳化反应能够完成,而且VC颗粒不易长大,原位生成小于0。
3.
Studies of microstructure on the coating by scanning electronic microscope(SEM),electron probe microzone analysis(EPMA) show that in-situ synthesis of TiB2 and TiB major ceramic phases disperse homogeneously in the γ-Co based alloy.
结果表明,涂层中原位生成的TiB2和TiB陶瓷颗粒相均匀分布在γ-Co基合金涂层中。
4)  in-situ growth
原位生长
1.
The effect of different additives,seeds and introduction methods on in-situ growth Columnar Crystals of alumina was summarized.
总结了国内外柱状晶增韧氧化铝陶瓷的技术,详细的介绍了各种添加剂、不同晶种及其引入方式对氧化铝原位生长柱状晶的影响,分析了柱状晶的生长机制,阐述了柱状晶增韧氧化铝陶瓷的途径与方法。
2.
By introducing ZrO2 micron powder into the thermit and through thermit combustion, liquid-liquid separation of metal/ceramics and crystal in-situ growth of eutectic reaction, self-toughening composite ceramics with in-situ growing nano-micron fibers were fabricated.
通过将ZrO2微米粉末引入铝热剂中,借助铝热燃烧、陶瓷/金属液相分离及共晶反应中的晶体原位生长,制备出原位生长纳微米纤维自增韧Al2O3/ZrO2陶瓷复合材料。
3.
The preparation process of structure and conducting channel in carbon nanotube field effect transistor (CNTFET) was reviewed, including AFM manipulation, CVD in-situ growth of single-walled carbon nanotube (SWCNT),AC dielectrophoresis and L-B manipulation, etc.
综述了碳纳米管场效应晶体管(CNTFET)的主要结构和导电沟道的制备工艺,如AFM探针操控、CVD原位生长、交流介电泳和L-B大面积操控排布等方法。
5)  in-situ [英][,ɪn 'sɪtju:]  [美]['ɪn 'sɪtju]
原位自生
1.
Progress in research on in-situ titanium matrix composites;
原位自生钛基复合材料的研究进展
2.
Study of different magnesium or silicon content on microstructures in in-situ Mg_2Si/Al alloy composites;
不同Mg、Si含量的原位自生Mg_2Si/A1基复合材料凝固组织的研究
3.
Study of Rare-earth as additon on ReinforcedSi Phase in-situ Zn-A1 Composites;
稀土对硅相增强原位自生Zn-Al复合材料的影响
6)  in-situ synthesis
原位自生
1.
Sliding wear behaviors of in-situ synthesis TiC/Ni60A composite coatings by argon arc cladding;
氩弧熔敷原位自生TiC/Ni60A复合涂层的滑动磨损特性
2.
The Mg_2Si/AM60 magnesium matrix composites fabricated by in-situ synthesis and its semi-solid rheoforming were investigated in the dissertation.
复合材料的制备可分为外加复合法和原位生成法,与外加复合法相比,原位自生镁基复合材料的增强相在基体内反应生成,具有尺寸小、界面洁净无污染、热稳定性好、与基体相容性好及制备成本低等优点,已成为金属基复合材料中的一个重要发展方向。
补充资料:-戊内酯、3-甲基丁内酯、咖吗-戊内酯
CAS: 108-29-2
分子式: C5H8O2
分子质量: 100.12
沸点: 207-208℃
熔点: -31-208℃

中文名称: 4-戊内酯、γ-戊内酯、3-甲基丁内酯、咖吗-戊内酯

英文名称: dihydro-5-methyl-2(3H)-Furanone、dihydro-5-methyl-2(3h)-furanon、4-hydroxypentanoic acid lactone、4-hydroxyvaleric acid lactone、4-methyl-gamma-butyrolactone、gamma-methyl-gamma-butyrolactone、gamma-valerolakton

性质描述: 无色至微黄色液体。凝固点-31℃,沸点205-206.5℃,83-84℃(1.73kPa),相对密度(25/25℃)1.0578,折光率(nD25)1.4301。能与水、许多有机溶剂、树脂和蜡等混溶。10%水溶液的pH为4.2。

生产方法: 由不饱和羧酸通过闭环反应来合成,例如乙酰乙酸与硫酸共热,或乙酰丙酸在镍、铜等催化剂存在下加氢。

用途: γ-戊内酯有较强的反应能力,可用作树脂溶剂及各种有关化合物的中间体。也用作润滑剂、增塑剂、非离子型表面活性剂的胶凝剂、加铅汽油的内酯类添加剂,用于纤维素酯和合成纤维的染色。γ-戊内酯具有香兰素和椰子香味。我国GB2760-86规定为允许使用的食用香料。主要用以配制桃、椰子、香草等型香精。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条