1) cerium sulfate supported on solica gel
硅胶固载硫酸铈
1.
Synthesis of butyl propionate catalyzed by cerium sulfate supported on solica gel;
硅胶固载硫酸铈催化合成丙酸丁酯
2.
By using cerium sulfate supported on solica gel as the catalyst,hexyl hexanoate was synthesized.
采用自制的硅胶固载硫酸铈为催化剂合成了己酸己酯,考察了催化剂用量、醇酸物质的量比、反应时间及带水剂用量等因素对收率的影响。
2) Ce2(SO4)3/SiO2
硅胶负载硫酸铈
3) gallium sulfate supported on silica gel
硅胶固载硫酸镓
1.
The catalytic activity of gallium sulfate supported on silica gel in synthesizing isoamyl hexanoate was studied.
采用自制的硅胶固载硫酸镓为催化剂合成了己酸异戊酯。
2.
Objective To study the catalytic activity of gallium sulfate supported on silica gel in the synthesis of amyl hexanoate.
目的研究硅胶固载硫酸镓在合成己酸戊酯工艺中的催化性能。
4) gallium sulfate supported on solica gel
硅胶固载硫酸镓
1.
Isoamyl butyrate was synthesized by using gallium sulfate supported on solica gel as the catalyst.
以自制的硅胶固载硫酸镓为催化剂,正丁酸和异戊醇为原料合成了丁酸异戊酯。
5) Fe2(SO4)3/SiO2
硅胶负载硫酸铁
1.
2-heptyl-1,3-dioxolane was synthesized from n-octylaldehyde and ethylene glycol using by Fe2(SO4)3/SiO2 as catalyst.
以正辛醛和乙二醇为原料,以硅胶负载硫酸铁[Fe2(SO4)3/SiO2]为催化剂,合成了2-庚基-1,3-二噁戊烷,考察了醛醇摩尔配比、反应时间、催化剂用量及其稳定性对产率的影响。
2.
Cinamaldehyde glycol acetal was synthesized from cinamaldehyde and ethylene glycol by using ferric sulphate-loaded silica gel(Fe2(SO4)3/SiO2) as catalyst.
以肉桂醛和乙二醇为原料,以硅胶负载硫酸铁(Fe2(SO4)3/SiO2)为催化剂,合成了肉桂醛乙二醇缩醛,考察了醛醇比(物质的量之比)、反应时间、催化剂用量及其稳定性对产率的影响。
6) La2(SO4)3/SiO2
硅胶负载硫酸镧
补充资料:硫酸铈(Ⅳ)
分子式: Ce(SO4)2
CAS号:
性质:黄色晶状粉末。溶于水。在酸性溶液中具很强的氧化性。高于450℃时分解。氢氧化铈(Ⅳ)溶于硫酸中制得。重要的水合物为四水合物。四水硫酸铈为黄色晶体,四方反棱柱体结构。双晶(其一与铀的类似的化合物同构,另一与锆的类似化合物同构)。溶于稀硫酸中。在水中分解。高于180℃时分解。350℃时生成硫酸铈酰(CeOSO4)。用于制取其他铈化合物。