1)  poly (vinyl chloride) /methylnethacrylacte-butadiene-styrene blend
PVC/MBS共混物
2)  MBS/PVC copolymer resin
MBS/PVC共聚树脂
1.
Relative average molecular weight and distribution of PVC mixed MBS/PVC copolymer resin was determined by Gel Permeation Chromatography.
采用GPC(凝胶渗透色谱)测定了MBS/PVC共聚树脂中PVC的相对分子质量及其分布,考察了样品质量浓度在0。
3)  PVC/ABS blend
PVC/ABS共混物
1.
The effect of plasticizer dioctyl phthalate(DOP) on the mechanical properties and shore A handness of PVC (SG-3,SG-5) and PVC/ABS blend were stuided.
研究了增塑剂DOP对聚氯乙烯(商品牌号SG-3,SG-5)及PVC/ABS共混物力学和硬度等性质的影响及其机理。
4)  PVC/SAN blends
PVC/SAN共混物
1.
Effect of AN content on the compatibility of PVC/SAN blends;
AN含量对PVC/SAN共混物相容性的影响
5)  PMSQ/PVC blends
PMSQ/PVC共混物
6)  ABS/PVC blends
ABS/PVC共混物
1.
The mechanical and theological properties of ABS/PVC blends are studied and the effects of compatibilizer α-SAN on the mechanical properties of ABS/PVC alloy are also discussed.
本文研究了ABS/PVC共混物的物理力学性能和加工流动性,并讨论了相容剂α-SAN对ABS/PVC共混物力学性能的影响。