2) complexing-precipitate
络合沉淀
1.
Preparation of high purity nano-TiO_(2) particles by complexing-precipitate method in IS-RPB;
络合沉淀法制备高纯纳米二氧化钛
2.
In this paper complexing-precipitate and the membrane integration technique was combined to treat wastewater containing cyanide in Lanzhou Petrochemical Industrial Factory.
以兰州石化氰化钠生产企业生产排放废水处理为研究对象,探讨了不同处理工艺的可行性,经过综合比较确定了络合沉淀与膜集成技术组合的处理工艺。
3) complex precipitation method
络合沉淀法
1.
Synthesis of Y_2O_3:Yb,Er nanocrystals by complex precipitation method and its up-conversion luminescence properties;
络合沉淀法合成纳米Y_2O_3:Yb,Er及其上转换发光性能
2.
Y2O2S∶Tb nanosized X-ray phosphors were prepared by complex precipitation method using EDTA and urea as chelating and precipitating agents,respectively.
以EDTA为螯合剂、尿素为沉淀剂,采用络合沉淀法制备了Y2O2S:Tb纳米X射线发光粉。
4) complex coprecipitation
络合共沉淀
1.
Homogeneous and well-crystallized nano-ZrO_(2)(Y_(2)O_(3)) powders were prepared by complex coprecipitation using a complex compound of H_(2)O_2.
采用过氧化氢络合共沉淀工艺制备Y ZrO2纳米粉体。
2.
Homogeneous and well-crystallized nano- ZrO_2(Y_2O_3) powders were prepared by complex coprecipitation using a complex compound of H_2O_2.
以氯氧化锆和氧化钇为原料,氨水为沉淀剂,采用过氧化氢络合共沉淀工艺制备Y-ZrO_2纳米粉体,得到含-OH与-OOH两种配位基团的过氧化锆酸沉淀。
6) compleximetry-precipitation method
络合-沉淀法
补充资料:氨基酸络合铜
分子式:
分子量:
CAS号:
性状:灰黑色粉末。无臭。
溶解情况:微溶于水,不溶于乙醇、乙醚、氯仿。
用途:营养性饲料添加剂,可满足动物对铜元素的需要
制备或来源:将蛋白质水解成复合氨基酸,然后与无机铜盐通过络核反应制得。
类别:矿物质类
分子量:
CAS号:
性状:灰黑色粉末。无臭。
溶解情况:微溶于水,不溶于乙醇、乙醚、氯仿。
用途:营养性饲料添加剂,可满足动物对铜元素的需要
制备或来源:将蛋白质水解成复合氨基酸,然后与无机铜盐通过络核反应制得。