1)  heterogeneous nucleation
非均匀形核
1.
Barium titanate based PTC ceramics doped by Nb-Si-Mn heterogeneous nucleation surface deposition method;
铌硅锰非均匀形核表面淀积掺杂PTC陶瓷
2.
Study on the heterogeneous nucleationof CaO/Al2O3/SiO2 system glasses;
CaO/Al_2O_3/SiO_2 系玻璃非均匀形核的研究
3.
For the homogeneous mixing of BaTiO_3(BT) powders with dopants and the exact control of the microstructures,phases and electrical properties of materials,a heterogeneous nucleation method was used to coat dopant Y(OH)_3 on the surface of nano-crystallized hydrothermal BT powders.
为实现改性杂质与钛酸钡粉体的均匀混合,达到对材料微结构、相结构和电学特性的准确控制,对水热纳米晶钛酸钡粉体进行了改性杂质的非均匀形核表面淀积包覆。
2)  Non-uniform Kernel
非均匀核
3)  heterogeneous nucleation surface coating process
非均匀形核表面包覆
1.
Preparation methods of BaTiO3-based PTC ceramic powder with surface modifying techniques (particle surface modifying method; citrate solution-liquid phase coating method; polyacrylamide gel-liquid phase coating method and so on) were introduced,especially the principle,characteristic,research status and applied prospect of heterogeneous nucleation surface coating process.
重点介绍BaTiO3基PTC瓷粉非均匀形核表面包覆制备的原理、特点、研究现状和应用前景。
4)  heterogeneous nucleation
非均匀成核
1.
Ferrite MgFe2O4 coated carbonyl iron composite powder was prepared by heterogeneous nucleation combined with the liquid deposition method to improve the oxidation resistance performance of carbonyl iron powder.
采用非均匀成核和化学沉淀相结合的方法制备了MgFe2O4铁氧体原位包覆羰基铁超细复合粉体,对制备工艺及其抗氧化性能进行了研究。
2.
Al_2O_3 nanosized composite powders encapsulated by ZrO_2(3Y) were prepared by heterogeneous nucleation combined with the co-deposition and were molded by dry pressing.
用非均匀成核法和液相共沉淀法相结合的方法制得ZrO2(3Y)包裹Al2O3纳米复合粉体,经干压成型,常压烧结制备ZTA复相陶瓷。
3.
ZrO_2(3Y)encapsulated Al_2O_3 nano composite powders were prepared by heterogeneous nucleation combined with the liquid co-deposition method using pH buffer solution as precipitator.
以pH值缓冲溶液为沉淀剂,用非均匀成核和液相共沉淀相结合的方法合成出了ZrO2(3Y)包裹Al2O3纳米复合粉体。
5)  heterogeneous reactor
[核]非均匀堆
6)  non-homogeneous nucleation
非均匀核化
1.
The homogeneous nucleation and the non-homogeneous nucleation of argon vapor molecules in the process of condensation were studied by molecular dynamic simulation.
本文运用分子动力学模拟方法对氩蒸气的均匀核化和非均匀核化进行了研究。