1) plasma boriding
等离子渗硼
1.
In order to improve the properties of hot work steel H 13 and prolong the working life of moulds,surface mechanical attrition treatment (SMAT) was combined with plasma boriding.
为了提高热作模具钢H13的性能,延长模具的使用寿命,本试验将表面机械研磨(SMA)处理与等离子渗硼相结合。
2.
The results showed that plasma boriding at 700 ℃ for 6 h,on the deformation-surface,the thickness and the hardness of the boronizing layer obviously increased,and the hardness gradient was smoother.
运用金相显微、X射线衍射分析(XRD)等技术研究表面机械研磨(SMAT)处理后低碳钢辉光膏剂等离子渗硼行为。
3.
In order to improve the properties of hot work steel H13 and prolong the working life of moulds,surface mechanical attrition treatment(SMAT)was combined with plasma boriding.
为了提高热作模具钢 H13的性能,延长模具的使用寿命,本试验将表面机械研磨(SMA)处理与等离子渗硼相结合。
2) Low Temperature Plasma-assisted Boriding
等离子低温渗硼
3) Iontophoresis
[ai,ɔntəfə'ri:sis]
离子等渗
5) plasma nitriding
等离子渗氮
1.
Influence of shot-peening on plasma nitriding of H13 steel;
喷丸对H13钢等离子渗氮处理的影响
2.
Influence of plasma nitriding surface modifications of titanium implant on bacterial adherence
等离子渗氮表面处理对纯钛材料细菌黏附能力的影响
3.
DC-pulsed plasma nitriding has been developed into an important technique for strengthening metallic materials.
脉冲直流等离子渗氮处理已成为金属材料表面强化的重要方法。
6) plasma chromizing
等离子渗铬
1.
The first plasma chromizing is achieved on cheaper low carbon steel surface and formed high chrome layer.
利用铬是碳化物形成元素且与α-Fe无限互溶的条件,在廉价低碳钢或中碳钢表面进行等离子渗铬,形成表面高铬合金层,当表面含铬量达到40%以上并在一定范围内渗层成分呈平缓的梯度分布时,再进行等离子渗碳,形成高铬高碳合金层。
补充资料:渗硼
分子式:
CAS号:
性质:渗镀品种之一,欲渗入的元素为硼。渗硼方法有固体粉末渗硼、气体渗硼、电解盐浴和盐浴的液体渗硼。渗硼层有优异的耐磨性、较好的耐蚀性和抗高温氧化性。例如钻井设备的泥浆泵零件,冲压、拉丝等模具经渗硼后可提高使用寿命。