1) coking chamber
炭化室
1.
In order to solve the problem of over-campaign service of No1 coke oven,the falling off of cover top brick at combustion chamber of flues 1-4 at the machine side of coking chamber and the big resistance of pushing on coke,the author adopts local patch and repair technology for north and south walls at the machine side of the coking chamber.
针对1#焦炉超龄服役,炭化室机侧1-4火道燃烧室盖顶砖脱落、推焦阻力大等现状,采用局部挖补技术对炭化室机侧南北墙进行修复,介绍了修复措施和实施方案。
2) carbonization chamber
炭化室
1.
A new coke oven maintenance method and a special sealing material for coke oven\'s carbonization chamber are introduced.
介绍了一种焦炉炭化室新型维修方法和焦炉炭化室专用密封材料。
2.
Some problems concerning the carbonization chambers of the coke oven and their remedy scenarios are introduced.
介绍了几孔焦炉炭化室存在的问题及修补维护情况,探讨了墙面修补和炉温特殊控制的相关方法,并提出解决焦炉使用后期推焦困难的措施。
3) wide oven chamber
宽炭化室
5) carbonizing stove
炭化烘焙室
6) chamber height
炭化室高度
补充资料:焦炉炭化室墙的火焰焊补
焦炉炭化室墙的火焰焊补
5矿。焦炉炭化窒墙蜘火嬲埠补
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条