2) low silicon and low carbon
低硅低碳
3) low carbon low silicon steel
低碳低硅钢
1.
The main problems of low carbon low silicon steel during the early time in the medium-thin slab caster in the No.
济钢第三炼钢厂利用中薄板连铸机生产低碳低硅钢的初期,主要存在钢水成分控制和可浇性的问题。
4) low carbon and low silicon steel
低碳低硅钢
1.
The porduction process of low carbon and low silicon steel Q195-1 is introduced and factors affecting compositions of the steel and counter measures analyzed and it is pointed out that the key to control the compositions of the steel is to control w(C) content in steel at the end-point within the limit of 0.
介绍了Q195-1低碳低硅钢的生产工艺,分析了影响其成分的因素及控制措施,指出将终点钢水w(C)准确控制在0。
2.
The process route of BOF-CC-high speed rolling for production of H08 steel, the typical low carbon and low silicon steel grade and practical production conditions are introduced.
介绍了低碳低硅钢的典型钢种—H0 8采用转炉、连铸和高线工艺的生产情况及工艺控制。