1) rapid densification
快速致密化
1.
SiCp/Fe composites are fabricated by an electric current heating dynamic process hot-pressing and rapid densification,which overcomes the limitations of powder metallurgy and casting.
研究了一种电流直加热动态热压快速致密化工艺,采用此工艺克服了粉末冶金法和铸造法的局限性,快速制备了10vol%SiCp/Fe复合材料,考察了材料在不同烧结电压和不同烧结时间情况下的致密化行为及其力学性能,结果表明此工艺制备的10vol%SiCp/Fe复合材料,相对密度达到99。
2.
The fundamental reasons of the rapid densification of the process are briefly discussed.
文中介绍了这一快速致密化技术的基本原理、方法特点 ;分析了该技术快速致密化的根本原因 ;概述及探讨了国内外对该技术在工艺及模拟方面的研究现状及存在的问题 ;最后展望了液相气化致密技术的应用前景。
3.
The status of research on chemical vapor infiltration for the rapid densification of C/C composites is reviewed and some problems in the research of the processings are pointed out.
简要概述了几种快速致密化技术的模拟研究进展。
2) rapid densification technology(RDT)
快速致密化工艺
3) rapid densification
快速致密
4) quickly densification mechanism
超快速致密化机理
5) pykno-
①快速 ②致密,浓缩
6) densification rate
致密化速率
1.
The influences of grain size and heating rates on the relationship of densification rates with the relative density were analyzed.
通过恒速升温方法研究了不同粒径及升温速率下α-Al2O3的烧结行为,着重分析了粒径及升温速率对α-Al2O3样品致密化速率与相对密度关系的影响。
2.
The maximal densification rates,being independent on the heating rates,occurred near the relative density of 73%.
通过对两种升温速率条件下样品致密化速率与相对密度关系曲线的比较可知,样品最大致密化速率均出现在相对密度73%左右,与升温速率无关。
补充资料:快速流态化
分子式:
CAS号:
性质:在流化床操作中,逐步提高气速,细粒子层经历固定床、散式膨胀床、鼓泡床、湍动床等状态,与此同时粒子的带出速率也在不断增加。在气速达到某一临界值时,床层密度急剧下降呈稀相。若要维持床密度不变,必须以等同于物料被吹出的速率将物料连续加至床层底部。这一操作区间称之为快速床。快速床内的连续相为稀相,同时存在有絮状的颗粒密集体(cluster),浓相密集体在快速床内不断上下交换。快速床技术已在石油催化裂化、矿石、氢氧化铝、纯碱的焙烧过程中使用。
CAS号:
性质:在流化床操作中,逐步提高气速,细粒子层经历固定床、散式膨胀床、鼓泡床、湍动床等状态,与此同时粒子的带出速率也在不断增加。在气速达到某一临界值时,床层密度急剧下降呈稀相。若要维持床密度不变,必须以等同于物料被吹出的速率将物料连续加至床层底部。这一操作区间称之为快速床。快速床内的连续相为稀相,同时存在有絮状的颗粒密集体(cluster),浓相密集体在快速床内不断上下交换。快速床技术已在石油催化裂化、矿石、氢氧化铝、纯碱的焙烧过程中使用。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条