1) Ammonia synthesis catalyst
合成氨催化剂
1.
This paper introduces the nanometer being preparation of the active components in the ammonia synthesis catalyst and its prospect.
文章介绍了合成氨催化剂中活性组分的纳米化制备与展
2) ammonia synthesis catalyst
氨合成催化剂
1.
Preparation and performance of ruthenium ammonia synthesis catalysts supported on cylinder-shaped activated carbon;
圆柱状成形Ru/AC氨合成催化剂制备及性能
2.
Study on mechanical strength of FeO-based ammonia synthesis catalyst;
FeO基氨合成催化剂的机械性能研究
3) A301 ammonia synthesis catalyst
A301氨合成催化剂
1.
The irregular A301 ammonia synthesis catalyst is spheroidized by means of shape factor and equivalent diameter.
对于不规则形状A301氨合成催化剂,测定了其形状系数和球化的当量直径及高压下本征动力学方程,用SPSR法测定了不规则催化剂颗粒的曲折因子,根据多组分单一反应等温球形A301氨合成催化剂内反应-扩散-维模型,用正交配置法结合解非线性方程组的Broyden拟牛顿法求解了模型,获得了催化剂粒内各组分的浓度分布和催化剂的内扩散有效因子。
4) ammonia synthesis A301 catalyst
氨合成A301催化剂
5) A203 type low temperature ammonia synthesis catalyst
A203型低温氨合成催化剂
6) ammonia synthesis catalyst ZA-5
ZA-5型氨合成催化剂
补充资料:铁系氨合成催化剂
分子式:
CAS号:
性质:合成氨工业生产中普遍采用的一种催化剂。主要组分是四氧化三铁。一般以精选天然磁铁矿为原料,除铁组分外,还含有能对催化反应起促进作用的添加物,一般是铝、钾、钙、镁等元素的氧化物,称为促进剂或助催化剂。此外,催化剂还含有极少量随原料或制作过程中引入的杂质硅、钛、硫、磷和氯等。用电阻炉或感应炉将天然或合成磁铁与添加物熔融、再经冷却、破碎至适宜粒度即得产品。催化剂在使用前,必须用含氢、氮的合成气进行还原变成多孔、活性高的α-Fe晶粒。正常操作温度范围为425~525℃。市场上也有预还原的催化剂品种。
CAS号:
性质:合成氨工业生产中普遍采用的一种催化剂。主要组分是四氧化三铁。一般以精选天然磁铁矿为原料,除铁组分外,还含有能对催化反应起促进作用的添加物,一般是铝、钾、钙、镁等元素的氧化物,称为促进剂或助催化剂。此外,催化剂还含有极少量随原料或制作过程中引入的杂质硅、钛、硫、磷和氯等。用电阻炉或感应炉将天然或合成磁铁与添加物熔融、再经冷却、破碎至适宜粒度即得产品。催化剂在使用前,必须用含氢、氮的合成气进行还原变成多孔、活性高的α-Fe晶粒。正常操作温度范围为425~525℃。市场上也有预还原的催化剂品种。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条