1) iron acetylacetonate
乙酰丙酮铁
1.
The polymerization of isoprene with iron acetylacetonate(Fe)/triisobutylaluminum(Al)/dialkyl phosphite(DP) catalyst was examined with respect to the effects of different dialkyl phosphites (methyl,ethyl,n-butyl and iso-octyl),the ratios of the catalyst components,polymerization temperature and time.
以乙酰丙酮铁 (简称Fe) /三异丁基铝 (简称Al) /亚磷酸二烷基酯 (简称DP)为催化体系 ,对异戊二烯进行聚合 ,考察了不同DP(烷基为甲基、乙基、正丁基或异辛基 )、催化剂组成及反应条件对聚合的影响。
4) Iron(Ⅲ) acetylacetonate
乙酰丙酮铁
1.
Iron(Ⅲ) acetylacetonate [Fe(acac) 3] was used as catalyst for the ring-opening polymerization of D,L-lactide and copolymerization of D,L-lactide with polyethylene glycol (PEG).
以乙酰丙酮铁 [Fe(acac) 3]为催化剂进行D ,L 丙交酯的开环聚合及在聚乙二醇 (PEG)存在下的开环共聚 ,研究了催化剂用量、反应温度和反应时间对聚合反应的影响以及PEG用量对共聚反应的影响 ,并探讨了丙交酯开环聚合机理 。
2.
The modified methylaluminoxane (MMAO) activated iron(Ⅲ) acetylacetonate (Fe(acac)_3)/diethyl phosphite (DEP) catalyst was examined in isoprene polymerization at 50 ℃, with respect to the effects of the amount of MMAO and DEP, the type of aluminum compound and solvent.
研究了改性甲基铝氧烷(MMAO)为助催化剂的乙酰丙酮铁(Fe(acac)3)/二乙基亚磷酸酯(DEP)催化剂作用下的异戊二烯(IP)聚合。
5) ferric triacetylacetonate
三乙酰丙酮铁
6) (acetylacetonato)iron(iii)
乙酰丙酮酸铁(III)
补充资料:乙酰丙酮铁
分子式:
CAS号:
性质:又称三乙酰丙酮铁。常温下为红棕色有光泽的结晶或玫瑰色结晶性粉末。熔点180~182℃(分解)。密度1.34g/cm3。溶于乙醇、乙醚、三氯甲烷和苯,微溶于水。它是由FeCl3.6H2O水溶液、乙酰丙酮甲醇溶液和CH3COONa水溶液分两步反应而制得。主要用作催化剂和促进剂。例如在聚氨酯推进剂中可用它作固化催化剂。
CAS号:
性质:又称三乙酰丙酮铁。常温下为红棕色有光泽的结晶或玫瑰色结晶性粉末。熔点180~182℃(分解)。密度1.34g/cm3。溶于乙醇、乙醚、三氯甲烷和苯,微溶于水。它是由FeCl3.6H2O水溶液、乙酰丙酮甲醇溶液和CH3COONa水溶液分两步反应而制得。主要用作催化剂和促进剂。例如在聚氨酯推进剂中可用它作固化催化剂。