说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 管件成形
1)  Tube forming
管件成形
2)  tube hydroforming
管件液压成形
1.
An Analysis on Numerical Simulation of Tube Hydroforming of Automobile;
基于数值模拟的汽车管件液压成形工艺分析
2.
To ensure the calculation precision and efficiency of the tube hydroforming process when using the dynamic explicit FEM,the effect of the virtual loading time was taken into account herein.
为保证管件液压成形动力显式有限元仿真的计算精度和提高计算效率,研究了虚拟加载时间对计算精度和计算效率的影响。
3.
This paper focuses on the characters of tube hydroforming,industrial applications and research of home and abroad.
管件液压成形技术作为汽车零件减重的重要方法之一 ,近几年发展很快 ,国外多个汽车公司已将其应用于管类零件的生产。
3)  external pressure forming of tubular part
管件外压成形
4)  Formation conditions
形成条件
1.
The formation conditions and explo-ration prospect of stratigraphic and lithologic oil-gas reservoirs of Jurassic in Junggar Basin;
准噶尔盆地侏罗系地层和岩性油气藏形成条件及勘探前景
2.
Characteristics of landslide distribution and formation conditions in Kangding County,Sichuan Province;
四川省康定县滑坡灾害发育特征与形成条件
3.
Geological disasters formation conditions and defensive trends;
地质灾害形成条件及其防治动向
5)  formative condition
形成条件
1.
This paper analyzed the formative conditions and control measures of natural gas hydrate in the course of oil and gas well surface test, and summari.
文中分析了地面测试过程中天然气水合物的形成条件和控制措施,并结合这些控制措施在川渝气田的实际应用效果,进行了综合分析和总结,对今后地面流程测试工艺中针对水合物方面的设计、施工和地面流程本身做进一步改进提供了一定的依据。
2.
rocky clint type,intrastratal type and earth cave or earth pit type are divided based on their formative conditions,and the engineering properties of different types of the soft soil are analysed together with the data investigated and tested by the author himself and others in this paper.
根据岩溶红土地基软土的形成条件划分出了岩沟型、层间型及洞中型三种不同的软土类型,在此基础上,通过取样测试并结合前人已有成果,对不同类型软土的工程地质特性进行了分析。
3.
his paper studies the formative conditions, formative process, sectional features,physical and chemical properties of wild walnut forest soils in the sole wild walnut nature reserve of our country.
本文研究了我国唯一的野核桃自然保护区的野核桃林土壤的形成条件、形成过程、剖面特征及理化特性。
6)  component shaping
工件成形
1.
Using the reversible multilevel-speed electromagnetic stirrer,the slurry transfer tool and its coater,the thin plate sample with five steps and the rheocasting mould,all of which are independently developed,a new rheoforming processing of Al alloy with slurry preparation systems and component shaping systems apart was exploited.
采用自主研制的双向多级速电磁搅拌装置、浆料转移工具和涂料、阶梯板流变性能试件和半固态合金压铸模具,开发出一种半固态合金浆料制备系统与工件成形系统分离的铝合金流变成形技术。
补充资料:主要射出成形材料成形时应注意事项

■主要射出成形材料成形时应注意事项
品  名 注    意    事    项
PVC
聚氯乙烯
1.  产品种类范围非常广(硬质、软质、聚合物等),成型条件各有不同,从熔融至分
解之温度范围很小,尤须注意加热温度。
2. 附着水分少,但成型周期尽可能减少(50℃~60℃热风干燥)。
3. 成型机方面,与材料直接接触的部位须电镀或采用不锈钢以防热分解所产生的盐酸
侵蚀。射出压力2100kg/cm2程度。
4. 所有塑料当中必须是细心注意温度调节。
5. 浇口附近易产生流纹,故射出操作后,柱塞不要后退使浇口充分固化后再瞬间退后为宜。
6. 加热之初温不宜高,特别注意熔融情形。第二级加热温度较高,且尽可能使成形周
期缩短,比较安全。


PA
聚醯胺树脂
1. 成型温度比其它材料高,故采用油加热的成形机较适当。
2. 吸湿性大,必须充分干燥。水分对成型品的品质影响甚大(80℃热风干燥约5~6小时)。
3. 须退火以消除内部歪斜。
PP
聚丙烯
1.  同PE,但成形温度必须较高。熔融温度170℃,超过190℃则流动性大增,则毛边增加,
易产生接缝及凹入情形。


PC
聚碳酸脂
1. 吸湿性比尼龙小,但若有些微之水分存在则成型品产生其它色泽或气泡,故必须密封
干燥同时成形时也须预备干燥(120℃之温度4小时)。
2. 加热温度超过320℃时则产生热分解,成品变色,故特别注意温度调节,又成型时的温度调节也非常重要,须特别注意其最低温度、最低时间。
3. 须退火以消除内部歪斜(130℃~135℃,1小时程度为准)。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条