1) La2(SO4)3/SiO2
硅胶负载硫酸镧
2) Fe2(SO4)3/SiO2
硅胶负载硫酸铁
1.
2-heptyl-1,3-dioxolane was synthesized from n-octylaldehyde and ethylene glycol using by Fe2(SO4)3/SiO2 as catalyst.
以正辛醛和乙二醇为原料,以硅胶负载硫酸铁[Fe2(SO4)3/SiO2]为催化剂,合成了2-庚基-1,3-二噁戊烷,考察了醛醇摩尔配比、反应时间、催化剂用量及其稳定性对产率的影响。
2.
Cinamaldehyde glycol acetal was synthesized from cinamaldehyde and ethylene glycol by using ferric sulphate-loaded silica gel(Fe2(SO4)3/SiO2) as catalyst.
以肉桂醛和乙二醇为原料,以硅胶负载硫酸铁(Fe2(SO4)3/SiO2)为催化剂,合成了肉桂醛乙二醇缩醛,考察了醛醇比(物质的量之比)、反应时间、催化剂用量及其稳定性对产率的影响。
3) Ce2(SO4)3/SiO2
硅胶负载硫酸铈
4) potassium carbonate doped silica gel
硅胶负载碳酸钾
5) HNb_3O_8·H_2O/SiO_2
硅胶负载铌酸
1.
Synthesis of α-D-glucose Pentaaccetate on HNb_3O_8·H_2O/SiO_2 Catalyst
微波辐射无溶剂体系中硅胶负载铌酸催化合成α-D-葡萄糖五乙酸酯
6) cerium sulfate supported on solica gel
硅胶固载硫酸铈
1.
Synthesis of butyl propionate catalyzed by cerium sulfate supported on solica gel;
硅胶固载硫酸铈催化合成丙酸丁酯
2.
By using cerium sulfate supported on solica gel as the catalyst,hexyl hexanoate was synthesized.
采用自制的硅胶固载硫酸铈为催化剂合成了己酸己酯,考察了催化剂用量、醇酸物质的量比、反应时间及带水剂用量等因素对收率的影响。
补充资料:硫酸镧
分子式:La2(SO4)3
CAS号:
性质:无水硫酸镧易吸水。可溶于水,溶解度随温度升高而下降,因而易重结晶。有无水硫酸镧和水合硫酸镧(含有结晶水)之分。在20℃的100g水中可溶解La2(SO4)3·8H2O 3.8g。含有结晶水的硫酸镧为六方晶系。硫酸镧在1000℃左右可热分解为三氧化二镧。用氧化镧与过量的浓硫酸反应、水合硫酸盐高温脱水可制得无水硫酸盐。把La2O3、La(OH)3或La2(CO3)3溶在稀H2SO4中可制得La2(SO4)3·8H2O。
CAS号:
性质:无水硫酸镧易吸水。可溶于水,溶解度随温度升高而下降,因而易重结晶。有无水硫酸镧和水合硫酸镧(含有结晶水)之分。在20℃的100g水中可溶解La2(SO4)3·8H2O 3.8g。含有结晶水的硫酸镧为六方晶系。硫酸镧在1000℃左右可热分解为三氧化二镧。用氧化镧与过量的浓硫酸反应、水合硫酸盐高温脱水可制得无水硫酸盐。把La2O3、La(OH)3或La2(CO3)3溶在稀H2SO4中可制得La2(SO4)3·8H2O。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条