1) MoS_2
MoS2
1.
MoS_2/WS_2 composite lubricating film was prepared by magnetron co-sputtering method.
采用磁控溅射共溅射法制备MoS2/W S2复合润滑薄膜,利用X射线衍射仪、X射线能谱仪及透射电子显微镜对薄膜的成分和结构进行分析,采用UMT-2MT型微摩擦磨损试验机在大气(相对湿度45%~50%)和室温(20~25℃)环境下评价薄膜的摩擦磨损性能。
2.
Four types of solid lubrication coatings containing MoS_2 were sprayed on the steel substrate by high velocity oxygen fuel(HVOF) spraying.
采用超音速火焰(HVOF)喷涂的方法在45钢表面制备四种含有MoS2的镍基固体润滑涂层,并研究了MoS2含量对涂层组织和性能的影响。
3.
The tribological behavior of the MoS_2 nanoparticles as additive in N46 machine oil was investigated on MM-200 ring-block tribometer.
由硫化钠和钼酸钠水溶液反应生成三硫化钼沉淀,将三硫化钼脱硫,制得了粒径为20~30 nm的纳米MoS2颗粒。
2) molybdenum disulfide
MoS2
1.
NH+4/molybdenum disulfide intercalated material was prepared by the exfoliation and restacking process.
以剥层重堆法制备了NH+4/MoS2插层复合物,该复合物可以作为长期储存的单层MoS2,同时也可作为先驱体以便插入其它客体分子制成新的插层复合物。
2.
Based on the exfoliation/restacking properties of LiMoS_2, several intercalation compounds of molybdenum disulfide with rich photic, electrical, magnetic, thermal and catalytical properties have been prepared.
MoS2为层状结构固体,基于LiMoS2的可剥离/重堆性,人们制备出了一系列MoS2的夹层化合物,这类材料具有丰富的光、电、磁、热、催化等性能。
3) MoS 2
MoS2
1.
MoS 2 crystals were synthesized by a hydrothermal method from Na 2MoO 4 and CS(NH 2) 2 under 160~220 ℃ for 24 h.
以硫脲为还原剂和硫源 ,利用水热法在 160~ 2 2 0℃下反应 ,合成了具有很好晶相的MoS2 。
2.
MoS 2/MoSi 2 in situ composites are produced by combustion synthesis with mechanical activation and pre heating.
采用活化燃烧合成法制备MoS2 /MoSi2 原位复合材料 ,用X -射线衍射仪 (XRD)对燃烧合成产物进行物相分析。
3.
Ni-MoS 2 self-lubricating composties are produced by means of hot-pressed technology.
用热压法生产Ni -MoS2 自润滑复合材料 ,研究了在微动摩擦条件下的室温和高温自润滑特性。
4) Ni MoS 2
Ni-MoS2
5) MoS2 soft coating
MoS2软涂层
6) (Ni-Co-P)-MoS_2
(Ni-Co-P)-MoS2